Please use this identifier to cite or link to this item: https://cris.library.msu.ac.zw//handle/11408/4358
Full metadata record
DC FieldValueLanguage
dc.contributor.authorMtangi, W.-
dc.contributor.authorSchmidt, M.-
dc.contributor.authorAuret, F. D.-
dc.contributor.authorMeyer, W. E.-
dc.contributor.authorJanse van Rensburg, P. J.-
dc.contributor.authorDiale, M.-
dc.contributor.authorNel, J. M.-
dc.contributor.authorDas, A. G. M.-
dc.contributor.authorDas, A. G. M.-
dc.contributor.authorLing, F. C. C.-
dc.contributor.authorChawanda, Albert-
dc.date.accessioned2021-06-04T08:48:55Z-
dc.date.available2021-06-04T08:48:55Z-
dc.date.issued2013-
dc.identifier.issn0021-8979-
dc.identifier.issn1089-7550-
dc.identifier.urihttps://aip.scitation.org/doi/10.1063/1.4796139-
dc.identifier.urihttps://doi.org/10.1063/1.4796139-
dc.identifier.urihttp://hdl.handle.net/11408/4358-
dc.description.abstractWe report on the space charge spectroscopy studies performed on thermally treated melt-grown single crystal ZnO. The samples were annealed in different ambients at 700 °C and also in oxygen ambient at different temperatures. A shallow donor with a thermal activation enthalpy of 27 meV was observed in the as-received samples by capacitance-temperature, CT scans. After annealing the samples, an increase in the shallow donor concentrations was observed. For the annealed samples, E27 could not be detected and a new shallow donor with a thermal activation enthalpy of 35 meV was detected. For samples annealed above 650 °C, an increase in acceptor concentration was observed which affected the low temperature capacitance. Deep level transient spectroscopy revealed the presence of five deep level defects, E1, E2, E3, E4, and E5 in the as-received samples. Annealing of the samples at 650 °C removes the E4 and E5 deep level defects, while E2 also anneals-out at temperatures above 800 °C. After annealing at 700 °C, the T2 deep level defect was observed in all other ambient conditions except in Ar. The emission properties of the E3 deep level defect are observed to change with increase in annealing temperature beyond 800 °C. For samples annealed beyond 800 °C, a decrease in activation enthalpy with increase in annealing temperature has been observed which suggests an enhanced thermal ionization rate of E3 with annealing.en_US
dc.language.isoenen_US
dc.publisherAmerican Institute of Physicsen_US
dc.relation.ispartofseriesJournal of Applied Physics;Vol. 113; No. 12-
dc.subjectPhysicsen_US
dc.subjectTemperaturesen_US
dc.subjectSingle crystal ZnO.en_US
dc.titleA study of the T2 defect and the emission properties of the E3 deep level in annealed melt grown ZnO single crystalsen_US
dc.typeArticleen_US
item.languageiso639-1en-
item.openairetypeArticle-
item.openairecristypehttp://purl.org/coar/resource_type/c_18cf-
item.fulltextWith Fulltext-
item.grantfulltextopen-
item.cerifentitytypePublications-
Appears in Collections:Research Papers
Files in This Item:
File Description SizeFormat 
Document1.pdfAbstract61.52 kBAdobe PDFView/Open
Show simple item record

Page view(s)

60
checked on Nov 29, 2024

Download(s)

22
checked on Nov 29, 2024

Google ScholarTM

Check


Items in MSUIR are protected by copyright, with all rights reserved, unless otherwise indicated.